Chlorinated polyvinyl chloride (CPVC) is a product obtained by chlorination modification of polyvinyl chloride (PVC), with a white or light yellow appearance, odorless and non-toxic powder or loose particles.
NO | item | technical requirement | |||||||||
R207 | R217 | R227 | R237 | R309 | R317 | R327 | R339 | R347 | R377 | ||
1 | Chlorine content(%)≥ | 66 | 66 | 66 | 66 | 68 | 66.5 | 66.5 | 68 | 66.5 | 66.5 |
2 | Density≥ (g/ml) | 0.55 | 0.5 | 0.5 | 0.55 | 0.5 | 0.55 | 0.5 | 0.55 | 0.5 | 0.55 |
3 | Volatile matter(%)≤ | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 |
4 | Impurity particle count≤ | 30 | 30 | 30 | 30 | 30 | 30 | 30 | 30 | 30 | 30 |
5 | whiteness(%)≥ (160ºC,10min | 70 | 70 | 70 | 70 | 70 | 70 | 70 | 70 | 70 | 70 |
6 | Vicat softening temperatureºC ≥ | 105 | 105 | 105 | 105 | 118 | 112 | 113 | 118 | 117 | 112 |
CPVC has superior high temperature resistance, corrosion resistance, flame retardancy, and rigidity, and is cost-effective compared to other thermoplastic plastics. Widely used in the manufacturing of various pipes, injection molded parts, plates, profiles, sheets, bars, etc.
The main application areas include:
(1) High temperature and corrosion-resistant pipes, fittings, valves, plates, sheets, and fillers for chemical towers used in chemical industry.
(2) Buried high-voltage power transmission cable protective sleeve.
(3) Pipes and fittings for hot and cold water.
(4) Materials for fire sprinkler pipelines and places with strict fire protection requirements.
(5) Process various components using CPVC rods.
20/25KG packaging, also customizable as needed.
During product transportation and loading and unloading, cleanliness should be maintained to prevent sun, rain, high temperature, and moisture, and to avoid damaging the packaging. It should be stored in a cool, dry, sun free warehouse with a temperature below 40 ºC for a storage period of two years. Two years later, after passing the performance test, it can still be used.