Customization: | Available |
---|---|
CAS No.: | 25133-97-5 |
Formula: | (C5h8o2.C5h8o2.C4h6o2)X |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
1. It has good compatibility with PVC and good dispersion. ACR and PVC resin molecular chains are entangled together, which promotes the melting and plasticization of PVC, effectively reduces the melting temperature of PVC, and improves the product quality on the basis of small energy saving. weather resistance;
2. Improve the fluidity of PVC materials, making it easier to form and extrude, ensuring the stability of long-term processing and forming;Testing items | Unit | Testing standards | 801 |
Prouduct appearance | -- | -- | White Powder |
surface density | g/cm³ | GB/T 1636-2008 | 0.45±0.10 |
Sieve residue (30 mesh) | % | GB/T 2916 | ≤2.0 |
Volatile matter | % | ASTM D5668 | ≤1.30 |
Intrinsic viscosity | -- | GB/T 1632-2008 | 3.50-6.00 |
KA-801 is widely used in PVC hard products, such as PVC profile, PVC pipe, PVC pipe fittings and PVC foam board and so on.
25Kg/package or as required by customers.
The product should be kept clean during transportation and handling, prevent sunshine, rain, high temperature and humidity, and avoid damage to packaging. It should be stored in a cool, dry, sunless warehouse with temperature below 40 C for two year. It can still be used after two year' performance test.1. Can you provide samples to customers for free?
Yes, we can provide free samples to help you with the test, but we need to charge the freight.