Specification | Unit | Test standard | KA-801 |
Appearance | -- |
-- |
White powder |
Bulk density | g/cm3 | GB/T 1636-2008 | 0.40±0.10 |
Sieve residue (30 mesh) | % | GB/T 2916 | ≤ 1.0 |
Volatile content | % | ASTM D5668 | ≤ 1.30 |
Intrinsic viscosity (q) | -- |
GB/T 16321 1-2008 | 12.00±1.00 |
Faster integration
Better melt fluidity
Excellent compressive resistance
Test Conditions: Melt Flow Rate Instrument Test Standard: ASTM D1238
melt flow rate(g/10min) | |
Test conditions | 210C 14. 1kg |
0# Control | 2.07 |
1# KA-401 | 2.59 |
KA-401 is widely used in PVC hard products, such as PVC profile, PVC pipe, PVC pipe fittings and PVC foam board and so on.
25Kg/package or as required by customers.
The product should be kept clean during transportation and handling, prevent sunshine, rain, high temperature and humidity, and avoid damage to packaging. It should be stored in a cool, dry, sunless warehouse with temperature below 40ºC for two year. It can still be used after two year' performance test.